Vestibulum ac Caloris Curatio Hastelloy B-2 Alloy.
by admin on 23-05-15
I: Calefacere Pro Hastelloy B-2 mixturas, magni momenti est servare superficiem mundam et immunem a contaminantibus ante et in calefactione. Hastelloy B-2 fragile fit si in ambitu sulphuris, phosphori, plumbi, vel aliis metallis liquescentis humilem contaminantibus calefit.
Read more
Corrosio resistentia Hastelloy
by admin on 23-05-15
Hastelloy est Ni-Mo admixtio carbidis et siliconis contento valde demissa, quae praecipitationem carbidum et alia incrementa in zonis pugillaribus et caloribus affectis minuit, ita ut bonum weldability etiam in iuncta statu minuat. Corrosio resistendi. Ut omnes novimus, H...
Read more
Hastelloy artifices resolvere commoda corrosionis-repugnantium mixturae productorum?
by admin on 23-05-15
Quae sunt commoda corrosioni-obsistentium admixtionum productorum corrosionum obsistentium admixtionum plerumque adhiberi non possunt in ambitibus corrosivis cum valida reducibilitate vel obsignatione alta (constantia anoxic) et exhibitio produ...
Read more
E-mail
E-mail
andrew@hnsuperalloys.com
Phone
Tel
+8618944814078
E-mail
E-mail
+8613661794406
Top
Intrare quaerere vel ESC claudere
English
French
German
Portuguese
Spanish
Russian
Japanese
Korean
Arabic
Irish
Greek
Turkish
Italian
Danish
Romanian
Indonesian
Czech
Afrikaans
Swedish
Polish
Basque
Catalan
Esperanto
Hindi
Lao
Albanian
Amharic
Armenian
Azerbaijani
Belarusian
Bengali
Bosnian
Bulgarian
Cebuano
Chichewa
Corsican
Croatian
Dutch
Estonian
Filipino
Finnish
Frisian
Galician
Georgian
Gujarati
Haitian
Hausa
Hawaiian
Hebrew
Hmong
Hungarian
Icelandic
Igbo
Javanese
Kannada
Kazakh
Khmer
Kurdish
Kyrgyz
Latin
Latvian
Lithuanian
Luxembou..
Macedonian
Malagasy
Malay
Malayalam
Maltese
Maori
Marathi
Mongolian
Burmese
Nepali
Norwegian
Pashto
Persian
Punjabi
Serbian
Sesotho
Sinhala
Slovak
Slovenian
Somali
Samoan
Scots Gaelic
Shona
Sindhi
Sundanese
Swahili
Tajik
Tamil
Telugu
Thai
Ukrainian
Urdu
Uzbek
Vietnamese
Welsh
Xhosa
Yiddish
Yoruba
Zulu
Kinyarwanda
Tatar
Oriya
Turkmen
Uyghur